參考文獻 |
[1] K.-N. Chen and K.-N. Tu, ”Materials challenges in three-dimensional integrated circuits,” MRS Bulletin, vol. 40, no. 03, pp. 219-222, 2015.
[2] K. N. Tu, ”Reliability challenges in 3D IC packaging technology,” Microelectronics Reliability, vol. 51, no. 3, pp. 517-523, 2011.
[3] K. N. Tu and T. Tian, ”Metallurgical challenges in microelectronic 3D IC packaging technology for future consumer electronic products,” Science China Technological Sciences, vol. 56, no. 7, pp. 1740-1748, 2013.
[4] A. Sazonov, D. Striakhilev, L. Czang-Ho, and A. Nathan, ”Low-Temperature Materials and Thin Film Transistors for Flexible Electronics,” Proceedings of the IEEE, vol. 93, no. 8, pp. 1420-1428, 2005.
[5] C. P. Wong, K.-S. Moon, and Y. Li, Nano-Bio- Electronic, Photonic and MEMS Packaging. Springer US, pp. XI, 761, 2010.
[6] 謝宗雍,「電子構裝技術簡介」,電子月刊第三卷第七期,p.57-p.76,1997年
[7] 徐祥禎,「電子構裝結構分析」,中華民國力學學會,2009年
[8] 田民波,「半導體電子元件構裝技術」,五男圖書出版股份有限公司,2008年
[9] 半導體製造概論,http://www.taiwan921.lib.ntu.edu.tw/mypdf/mf23.pdf
[10] K. N. Tu, Solder Joint Technology. Springer Verlag New York, pp. XVI, 370, 2007.
[11] M. Amagai, ”Characterization of chip scale packaging materials,” Microelectronics Reliability, vol. 39, no. 9, pp. 1365-1377, 1999.
[12] Y. Kim, S.-K. Kang, S.-D. Kim, and S. E. Kim, ”Wafer warpage analysis of stacked wafers for 3D integration,” Microelectronic Engineering, vol. 89, pp. 46-49, 2012.
[13] N. M. Poon, C. M. L. Wu, J. K. L. Lai, and Y. C. Chan, ”Residual shear strength of Sn-Ag and Sn-Bi lead-free SMT joints after thermal shock,” IEEE Transactions on Advanced Packaging, vol. 23, no. 4, pp. 708-714, 2000.
[14] X. Luhua and J. H. L. Pang, ”Effect of intermetallic and Kirkendall voids growth on board level drop reliability for SnAgCu lead-free BGA solder joint,” , 56th Electronic Components and Technology Conference 2006, p. 8, 2006.
[15] X. Ma, Y. Qian, and F. Yoshida, ”Effect of La on the Cu–Sn intermetallic compound (IMC) growth and solder joint reliability,” Journal of Alloys and Compounds, vol. 334, no. 1, pp. 224-227, 2002.
[16] 潘致弘,行政院勞工委員會勞工安全衛生研究所「鉛對健康危害預防手冊」,p2,2002年
[17] Q. Lin, Z. Jie, W. Xiu-min, and W. Lai, ”The effect of Bi on the IMC growth in Sn-3Ag-0.5Cu solder interface during aging process,” in Proceedings of 2004 International Conference on the Business of Electronic Product Reliability and Liability , pp. 42-46, 2004.
[18] G. Duscher, M. F. Chisholm, U. Alber, and M. Ruhle, ”Bismuth-induced embrittlement of copper grain boundaries,” Nat Mater, vol. 3, no. 9, pp. 621-626, 2004.
[19] Q. L. Yang and J. K. Shang, ”Interfacial segregation of Bi during current stressing of Sn-Bi/Cu solder interconnect,” Journal of Electronic Materials, vol. 34, no. 11, pp. 1363-1367, 2005.
[20] J. W. Morris, J. L. F. Goldstein, and Z. Mei, ”Microstructure and mechanical properties of Sn-In and Sn-Bi solders,” The Journal of The Minerals, journal article vol. 45, no. 7, pp. 25-27, 1993.
[21] J.-I. Lee, S.-W. Chen, H.-Y. Chang, and C.-M. Chen, ”Reactive wetting between molten Sn-Bi and Ni substrate,” Journal of Electronic Materials, vol. 32, no. 3, pp. 117-122, 2003.
[22] P. J. Shang, Z. Q. Liu, D. X. Li, and J. K. Shang, ”Bi-induced voids at the Cu3Sn/Cu interface in eutectic SnBi/Cu solder joints,” Scripta Materialia, vol. 58, no. 5, pp. 409-412, 2008.
[23] Q. K. Zhang, H. F. Zou, and Z. F. Zhang, ”Influences of Substrate Alloying and Reflow Temperature on Bi Segregation Behaviors at Sn-Bi/Cu Interface,” Journal of Electronic Materials, vol. 40, no. 11, p. 2320, 2011.
[24] M. Mccormack, H. S. Chen, G. W. Kammlott, and S. Jin, ”Significantly Improved Mechanical Properties of Bi- Sn Solder Alloys by Ag- Doping,” Journal of Electronic Materials, vol. 26, no. 8, pp. 954-958, 1997.
[25] Y. Maruya, H. Hata, I. Shohji, and S. Koyama, ”Bonding Characteristics of Sn-57Bi-1Ag Low-Temperature Lead-Free Solder to Gold-Plated Copper,” Procedia Engineering, vol. 184, pp. 223-230, 2017.
[26] H. Hata, Y. Maruya, and I. Shohji, ”Interfacial Reactions in Sn-57Bi-1Ag Solder Joints with Cu and Au Metallization,” Materials Transactions, vol. 57, no. 6, pp. 887-891, 2016.
[27] C. Fuchs, T. Schreck, and M. Kaloudis, ”Interfacial reactions between Sn–57Bi–1Ag solder and electroless Ni-P/immersion Au under solid-state aging,” Journal of Materials Science, vol. 47, no. 9, pp. 4036-4041, 2012.
[28] A. K. Gain and L. Zhang, ”Interfacial microstructure, wettability and material properties of nickel (Ni) nanoparticle doped tin–bismuth–silver (Sn–Bi–Ag) solder on copper (Cu) substrate,” Journal of Materials Science: Materials in Electronics, vol. 27, no. 4, pp. 3982-3994, 2016.
[29] S. K. Lin, T. L. Nguyen, S. C. Wu, and Y. H. Wang, ”Effective suppression of interfacial intermetallic compound growth between Sn–58 wt.% Bi solders and Cu substrates by minor Ga addition,” Journal of Alloys and Compounds, vol. 586, pp. 319-327, 2014.
[30] C. H. Chen, B. H. Lee, H. C. Chen, C. M. Wang, and A. T. Wu, ”Interfacial Reactions of Low-Melting Sn-Bi-Ga Solder Alloy on Cu Substrate,” Journal of Electronic Materials, vol. 45, no. 1, pp. 197-202, 2015.
[31] F. F. Tian and Z. Q. Liu, ”The interfacial microstructure and Kirkendall voids in In-48Sn/Cu solder joint,” 14th International Conference on Electronic Packaging Technology 2013, pp. 907-910, 2013.
[32] F. Tian, Z.-Q. Liu, P.-J. Shang, and J. Guo, ”Phase identification on the intermetallic compound formed between eutectic SnIn solder and single crystalline Cu substrate,” Journal of Alloys and Compounds, vol. 591, pp. 351-355, 2014.
[33] T. H. Chuang, K. W. Huang, and W. H. Lin, ”Mechanisms for the intermetallic formation during the Sn-20In-2.8Ag/Ni soldering reactions” Journal of Electronic Materials, vol. 33, no. 4, pp. 374-381, 2004.
[34] S. K. Lin, C. W. Hsu, S. W. Chen, and C. M. Hsu, ”Interfacial reactions in Sn–20In–2.8Ag/Cu couples” Materials Chemistry and Physics, vol. 142, no. 1, pp. 268-275, 2013.
[35] D. G. Kim, J. W. Yoon, C. Y. Lee, and S. B. Jung, ”Reaction diffusion and formation of Cu11In9 and In27Ni10 phases in the couple of indium-substrates” Materials Transactions, vol. 44, no. 1, pp. 72-77, 2003.
[36] S. Sommadossi, W. Gust, and E. J. Mittemeijer, ”Phase characterisation and kinetic behaviour of diffusion soldered Cu/In/Cu interconnections” Materials Science and Technology, vol. 19, no. 4, pp. 528-534, 2003.
[37] W. Keppner, R. Wesche, T. Klas, J. Voigt, and G. Schatz, ”Studies of compound formation at Cu-In, Ag-In and Au-In interfaces with perturbed γ-γ angular correlations,” Thin Solid Films, vol. 143, no. 2, pp. 201-215, 1986.
[38] M. Gossla, H. Metzner, and H.-E. Mahnke, ”Coevaporated Cu–In films as precursors for solar cells,” Journal of Applied Physics, vol. 86, no. 7, pp. 3624-3632, 1999.
[39] N. Takeo, M. Hiroshi, and B. Shigeru, ”Transition of Roughness Evolution in Cu–In Alloy Films by the Formation of Intermetallic Compounds,” Japanese Journal of Applied Physics, vol. 44, no. 4R, p. 1932, 2005.
[40] B. D. Cullity, Elements of X Ray Diffraction. BiblioBazaar, 2011.
[41] A. Parretta and A. Rubino, ”Kinetics of intermetallics transformation in sputtered Cu-In alloys studied by electrical resistance measurements,” Solid State Communications, vol. 96, no. 10, pp. 767-770, 1995.
[42] C. von Klopmann, J. Djordjevic, and R. Scheer, ”Real-time studies of phase transformations in Cu–In–Se–S thin films,” Journal of Crystal Growth, vol. 289, no. 1, pp. 113-120, 2006.
[43] F. Tian, Z.-Q. Liu, and J. Guo, ”Phase transformation between Cu(In,Sn)2 and Cu2(In,Sn) compounds formed on single crystalline Cu substrate during solid state aging,” Journal of Applied Physics, vol. 115, no. 4, pp. 043520, 2014.
[44] K. N. Subramanian, Ed. ”Lead-free electronic solders: A special issue of the journal of materials science: Materials in electronics. ” United States: Springer-Verlag New York Inc., 2007. |