LiCoO2 particles were coated with various wt.% of lanthanum aluminum garnets (3LaAlO(3):Al2O3) by an in situ sol-gel process, followed by calcination at 1123 K for 12 h in air. X-ray diffraction (XRD) patterns confirmed the formation of a 3LaAlO(3):Al2O3