The LiCoO2 cathode material was surface treated with the Li4Ti5O12 particles by a simple mechano-thermal process, followed by calcination at 723 K for 10 h in air. The X-ray diffractometer (XRD) patterns showed a single-phase hexagonal alpha-NaFeO2-type s