Pure aluminum (99.999%) cubes were polished by abrasive papers and then heated in a furnace at 873 K for 25 h in order to grow oxide on the polished surfaces, coded as Al/oxide. These Al/oxide samples were stacked with a pure Al cube and a Al-7 mass%Si cu