The length scale of heterogeneity in blends of poly(2,6-dimethyl-p-phenylene oxide) (PPO) with poly(a-methyl styrene) (PalphaMS) was investigated using solid state C-13 NMR. The PPO/PalphaMS blend system was homogeneous at ambient, but phase separation at