參考文獻 |
1.L. L. Liao, M. J. Dai, C. K. Liu, and K. N. Chiang, “Thermo-electric finite element analysis and characteristic of thermoelectric generator with intermetallic compound”, Microelectron. Eng., 120, 194-199 (2014).
2.G. Jeffrey Snyder and Eric S. Toberer, “Complex thermoelectric materials”, Nat. Mater., 7, 105-114 (2008).
3.S. W. Chen and C. N. Chiu, “Unusual cruciform pattern interfacial reactions in Sn/Te couple”, Scripta Mater., 56, 97-99 (2007).
4.M. L. Huang, T. Loeher, and A. Ostmann, and H. Reichi, “Role of Cu in dissolution of Cu metallization in molten Sn-based solders”, Appl. Phys. Lett., 86, 181908 (2005).
5.S. C. Hsu, S. J. Wang, and C. Y. Liu, “Effect of Cu content on interfacial reaction between Sn(Cu) alloys and Ni/Ti thin-film metallization”, J. Electron. Mater., 32, 1214-1221 (2003).
6.C. N. Liao and C. H. Lee, “Suppression of vigorous liquid Sn/Te reactions by Sn-Cu solder alloys”, J. Mater. Res., 23, 3303-3308 (2008).
7.C. N. Liao and Y. C. Huang, “Effect of Ag addition in Sn on growth of SnTe compound during reaction between molten solder and tellurium”, J. Mater. Res., 25, 391-395 (2010).
8.C. N. Chiu, C. H. Wang, and S. W. Chen, “Interfacial reactions in the Sn-Bi/Te couples”, J. Electron. Mater., 37, 40-44 (2007).
9.S. W. Chen, C. Y. Wu, H. J. Wu, and W. T. Chiu, “Interfacial reactions in Sn/Bi2Te3, Sn/Bi2Se3 and Sn/Bi2(Te1-xSex)3 couples”, J. Alloys Compd., 611, 313-318 (2014).
10.S. W. Chen, H. J. Wu, C. Y. Wu, C. F. Chang, and C. Y. Chen, “Reaction evolution and alternating layer formation in Sn/(Bi0.25Sb0.75)2Te3 and Sn/Sb2Te3 couples”, J. Alloys Compd., 553, 106-112 (2013).
11.W. H. Chao, Y. R. Chen, S. C. Tseng, P. H. Yang, R. J. Wu, and J. U. Hwang, “Enhanced thermoelectric properties of metal film on bismuth telluride-based materials”, Thin Solid Films, 570, 172-177 (2014).
12.Y. C. Lan, D. Z. Wang, G. Chen, and Z. F. Ren, “Diffusion of nickel and tin in p-type (Bi,Sb)2Te3 and n-type Bi2(Te,Se)3 thermoelectric materials”, Appl. Phys. Lett., 92 101910 (2008).
13.K. Xiong, W. Wang, H. N Alshareef, R. P Gupta, J. B White, B. E Gnade, and K. Cho, “Electronic structures and stability of Ni/Bi2Te3 and Co/Bi2Te3 interfaces”, J. Phys. D: Appl. Phys., 43, 115303 (2010).
14.Brenner, A., and Riddell, G. E, “Deposition of Nickel and Cobalt by chemical reduction”, J. Res., 39, 385-395 (1947).
15.R C Agarwala and V. Agarwala, “Electroless alloy/composite coatings: A review”, Sadhana, 28, 475-493 (2003).
16.P. Sahoo and S. K. Das, “Tribology of electroless nickel coatings – A review”, Mater. Des., 32, 1760-1775 (2011).
17.R. Parkinson, “Properties and applications of electroless nickel”, Nickel Development Institute Technical Series no.10081, 1, (1995).
18.S. L. Chow, N. E. Hedgecock, and M. Schlesinger, “Electron microscope study of the nucleation and growth of electroless cobalt and nickel”, Electrochem. Soc., 119, 1614-1619 (1972).
19.H. Ashassi-Sorkhabi and S. H. Rafizadeh, “Effect of coating time and heat treatment on structures and corrosion characteristics of electroless Ni-P alloy deposits”, Surf. Coat. Technol., 176, 318-326 (2004).
20.T. Y. Lin, C. N. Liao, and Albert T. Wu, “Evaluation of diffusion barrier between lead-free solder systems and thermoeletic materials”, J. Electron. Mater., 41, 153-158 (2012).
21.L. C. Lo and Albert T. Wu, “Interfacial reactions between diffusion barriers and thermoelectric materials under current stressing”, J. Electron. Mater., 41, 3325-3320 (2012).
22.P. Y. Chien, C. H. Yen, H. H. Hsu, and Albert T. Wu, “Polarity effect in a Sn3Ag0.5Cu/bismuth telluride thermoelectric system”, J. Electron. Mater., 43, 284-289 (2014).
23.C. F. Tseng, and J. G. Duh, “Correlation between microstructure evolution and mechanical strength in the Sn-3.0Ag-0.5Cu/ENEOIG solder joint”, Mater. Sci. Eng., A, 580, 169-174 (2013).
24.JEDEC JESD22-B117B-2014.
25.J. Y. Hon Chia, B. Cotterell, and T. C. Chai, “The mechanics of the solder ball shear test and the effect of shear rate”, Mater. Sci. Eng., 417, 259-294 (2006).
26.J. W. Kim, Y. C. Lee, S. S. Ha, and S. B. Jung, “Failure behaviors of BGA solder joints under various loading conditions of high-speed shear test”, J. Mater. Sci. – Mater. Electron., 20, 17-24 (2009).
27.J. W. Kim, D. G. Kim, and S. B. Jung, “Investigations of the test parameters and bump structures in the shear test of flip chip solder bump”, Thin Solid Films, 204, 405-409 (2006).
28.H. Okamoto, “Ni-P(nickel-phosphorus)”, J. Phase Equilib., 21, 210 (2000).
29.J. M. Koo and S. B. Jung,“Effect of substrate metallization on mechanical properties of Sn-3.5Ag BGA solder joints with multiple reflows”, Microelectron. Eng., 82, 569-574 (2005).
30.J. W. Yoon and S. B. Jung, “Interfacial reaction between Sn-0.4Cu solder and Cu substrate with or without ENIG plating layer during reflow reaction“, J. Alloys Compd., 396, 122-127 (2005).
31.Y. C. Lin, K. J. Wang, and J G. Duh, “Detailed phase evolution of phosphorous-rich layer and formation of the Ni-Sn-P compound in Sn-Ag-Cu/Electroplated Ni-P solder joints”, J. Electron. Mater., 39, 283-294 (2009).
32.P. Nash, "Phase diagrams of binary nickel alloys." ASM International(USA), 394, (1991).
33.E.A. Brandes and G B Brook., Smithells Metals Reference Book, Seventh ed., 1992.
34.林能億碩士論文,國立中央大學化學工程與材料工程研究所(2014). |