Nanosized NiCoB amorphous alloy catalysts with Co/Ni ratios varying from 0 to 3 were prepared by chemical reduction of nickel acetate and cobalt acetate with sodium borohydride in methanolic solution at room temperature under N-2 gas with vigorous stirrin