DC 欄位 |
值 |
語言 |
DC.contributor | 機械工程學系 | zh_TW |
DC.creator | 楊樺成 | zh_TW |
DC.creator | Hwa-sheng Yong | en_US |
dc.date.accessioned | 2015-7-29T07:39:07Z | |
dc.date.available | 2015-7-29T07:39:07Z | |
dc.date.issued | 2015 | |
dc.identifier.uri | http://ir.lib.ncu.edu.tw:444/thesis/view_etd.asp?URN=102323094 | |
dc.contributor.department | 機械工程學系 | zh_TW |
DC.description | 國立中央大學 | zh_TW |
DC.description | National Central University | en_US |
dc.description.abstract | 在這項研究中,鋁合金6066經過退火後深冷鍛造,再進行固溶處理和頂時效處理。深冷鍛造鋁合金與傳統的鋁合金6066-T6合金相比,深冷鍛造鋁合金在延展性增加35%,但在UTS和YS上卻犧牲了大約8%。陽極處理對於6066-T6有/無深冷鍛試片的抗腐蝕能力一併加以量測和討論。 | zh_TW |
dc.description.abstract | In this study, AA6066 alloy samples were cryogenically forged after annealing and then subjected to solution and aging treatments. Compared with conventional 6066-T6 alloy samples, the cryogenically forged samples exhibited a 35% increase in elongation but sacrificed about 8% in UTS and YS. The effect of anodization on the corrosion resistance of 6066-T6 with/without cryogenically-forged samples was also investigated, and the results are discussed in this study. | en_US |
DC.subject | 鋁合金6066-T6 | zh_TW |
DC.subject | 深冷鍛造 | zh_TW |
DC.subject | 析出物 | zh_TW |
DC.subject | 陽極處理 | zh_TW |
DC.subject | AA6066-T6 | en_US |
DC.subject | cryogenic forging | en_US |
DC.subject | precipitates | en_US |
DC.subject | anodized | en_US |
DC.title | 深冷變形與陽極處理對6066-T6機械性質的影響 | zh_TW |
dc.language.iso | zh-TW | zh-TW |
DC.title | Effect of Cryogenic deformation and anodized treatment on AA6066-T6 mechanical properties | en_US |
DC.type | 博碩士論文 | zh_TW |
DC.type | thesis | en_US |
DC.publisher | National Central University | en_US |