    题名: Refinement of the primary Si particles in hypereutectic aluminum alloy
    作者: 李雄;Hsu, Chang-Chuan;Wang, Jian-Yih;Huang, Jian-Jia;Lee, Shyong
    贡献者: 工學院機械工程學系
    关键词: Aluminum base alloys;Automotive engineering;Characterization and Evaluation of Materials;Chemistry and Materials Science;Coarsening;Engineering Thermodynamics;Heat and Mass Transfer;Intermetallic compounds;Machines;Magnetic Materials;Magnetism;Manufacturing;Materials Science;Metallic Materials;Plastic deformation;Processes;Reduction;Silicon;Solid Mechanics;Thermal expansion;Weight reduction;재료공학
    日期: 2012-08-01
    上传时间: 2026-04-23 15:25:26 (UTC+8)
    出版者: Korean Institute of Metals and Materials;Springer: The Korean Institute of Metals and Materials
    摘要: 摘要: Al-Si alloys, with such excellent properties as low weight, low thermal expansion coefficient, and high wear-resistance, are ideal materials for the automobile and aerospace industries. However, their applications have been hampered by the coarsening of the primary-Si particles in Al-Si alloys. In this study, simple plastic deformation was used to reduce primary-Si particles and to improve the wear-resistance and mechanical strength of Al-Si alloys. Experimental results showed that mechanical rolling decreased the grain size of primary-Si particles in Al-Si alloys and reduced the variation in silicon particle size. After 60%-roll-reduction, the alloy showed an improved tensile strength of 340 MPa, which is attributed to the work hardening of the aluminum matrix and the dispersion strengthening of the primary-Si particles. Data from wear-resistance testing showed that rolling led to a reduction in wear loss. This improvement in wear resistance is due to the particle size refinement of silicon at a high percentage-roll-reduction.
    其他題名: Met. Mater. Int
    出版者: Springer: The Korean Institute of Metals and Materials
    出版日期: 2012-08
    出處: Metals and Materials International, 2012, 18(4), , pp.567-571
    版權: The Korean Institute of Metals and Materials and Springer Netherlands 2012
    識別號: ISSN: 1598-9623
    識別號: EISSN: 2005-4149
    識別號: DOI: 10.1007/s12540-012-4003-1
    显示于类别:[機械工程學系] 期刊論文

    文件中的档案:

    档案 描述 大小格式浏览次数
    index.html0KbHTML14检视/开启


    在NCUIR中所有的数据项都受到原著作权保护.

    社群 sharing

    ::: Copyright National Central University. | 國立中央大學圖書館版權所有 | 收藏本站 | 設為首頁 | 最佳瀏覽畫面: 1024*768 | 建站日期:8-24-2009 :::
    DSpace Software Copyright © 2002-2004  MIT &  Hewlett-Packard  /   Enhanced by   NTU Library IR team Copyright ©   - 隱私權政策聲明